Practical Interpretation of Microstructures, 3 day, November 9-11, 2026

When:  Mon, Nov 9, 2026 from 08:30 to 16:30 (ET)

Practical Interpretation of Microstructures is a three-day course that combines lectures with hands-on microscopy practice to build skills in microstructural analysis. Students will work with microstructures from key alloy systems including steel, stainless steel, cast iron, titanium, copper, aluminum, superalloys, and other materials commonly seen in the field.

The course examines how microstructures change with different heat treatments and processing methods, including the differences between wrought and cast materials. Lectures are supported by examining real microstructures where important features are identified and discussed. Students will spend significant time at microscope stations examining about 60 prepared specimens, using an illustrated reference guide with detailed annotations.

No prerequisites are required, though having some background in sample preparation, heat treating, or metallurgy will enhance the understanding of the presented material.

Students are encouraged to bring their own prepared specimens for discussion during the course.

ENDORSED BY:

WHO SHOULD ATTEND?

  • Metallographers looking to strengthen their interpretation skills
  • Technicians working with microstructural analysis
  • Engineers who need to understand microstructures in their work
  • Individuals who are required to interpret microstructures

LEARNING OBJECTIVES

Upon completion of this course, you should be able to:

  • Apply correct terminology when describing microstructures
  • Correlate what is seen in microstructures to heat treatment, mechanical properties, and chemistry
  • Recognize martensite, austenite, bainite, and ferrite in ferrous alloys
  • Determine manufacturing processes based on indications in the microstructure
  • Identify structures of non-ferrous alloys such as super alloys, titanium, copper, and aluminum alloys
  • Analyze imperfections and their causes
  • Distinguish between preparation artifacts and actual microstructural features

COURSE OUTLINE:

  1. Proper Terminology for Describing Microstructures
  2. Optimizing the Images on the Metallograph
  3. Iron/ Carbon Phase Diagram and TTT Diagram
  4. Structures of Carbon and Alloy Steels as Produced by Heat Treatments
  5. Structures of Stainless Steels and Heat Resisting Alloys
  6. Microstructures of Titanium and Its Alloys
  7. Structures of Aluminum Alloys, Cast and Wrought
  8. Microstructures of Copper-Based Alloys
  9. Common Failure Modes of Various Alloys

Continuing Education Units: 3.0

This course satisfies one of the requirements for the Certificate of Achievement in Metallography.