Engineering Ordered Two-Dimensional Defect Phases to Strengthen Structural Alloys

When:  Thu, Nov 5, 2026 from 11:00 to 12:00 (ET)

Engineering ordered two-dimensional defect phases to strengthen structural alloys

Sponsored by The Heat Treating Society

Planar defects can host chemically and structurally distinct phases that influence resistance to deformation. These phases often develop during service, limiting control over their density and distribution. Here, we demonstrate how predeformation followed by aging creates dense networks of ordered defect phases before service in the single-crystalline CoNi-based γ/γ′ superalloy ERBOCo-4 and a polycrystalline CoCrW alloy.

In ERBOCo-4, predeformation introduces approximately 24 stacking faults per 450 nm γ′ precipitate. Subsequent aging promotes Co and W enrichment and local transformation into atomically thin D0₁₉- and D0₂₄-ordered structures. In CoCrW, aging enhances W segregation and produces thicker, coherent lamellae containing D0₁₉-ordered Co₃(Cr,W) segments and disordered hexagonal regions.

These architectures improve strength and creep resistance. In ERBOCo-4, room-temperature compressive strength increases by more than 200 MPa while retaining work hardening. At 750 °C and 800 MPa, the minimum creep rate decreases more than threefold and load-on strain is suppressed. CoCrW also exhibits reduced load-on strain and a lower steady-state creep rate at 750 °C and 400 MPa.

 Atomic-resolution scanning transmission electron microscopy, energy-dispersive X-ray spectroscopy and phase-field simulations identify local chemical ordering as a key strengthening contribution. The confined phases in ERBOCo-4 remain shearable while impeding slip transmission, whereas the thicker phases in CoCrW are associated with reduced work hardening. These findings establish thickness and confinement as central design parameters for balancing strengthening and shearability. Finally, we discuss extensions to other alloys and processing routes, including additive manufacturing.

SPEAKER: Andreas Bezold, Department of Materials Science and Engineering, Friedrich Alexander University Erlangen-Nuremberg