Industrial Computed Tomography for Metals Characterization, December 9, 2026

When:  Wed, Dec 9, 2026 from 08:30 to 16:30 (ET)

(New) Additive manufacturing has broken the traditional nondestructive testing rulebook. Internal channels, lattice structures, as-built surface roughness, and pores an order of magnitude smaller than those in castings or forgings defeat the surface-sensitive methods that industry has relied on for decades. X-ray computed tomography is the method that reaches into the volume — and increasingly, it is the method that qualification programs and emerging standards are built around.

This course teaches CT as a characterization tool for metals. Students learn where CT sits among the nondestructive methods, the physics and instrumentation that produce a CT volume, and how to specify a scan from the inspection question rather than from habit. Radiation safety practice around an industrial x-ray source is covered explicitly. Students then diagnose the artifacts that corrupt CT data — beam hardening, streaking, rings, truncation, and scatter.

In the laboratory session, students work on ASM's Nikon XT H 225 ST microfocus CT system and analyze the resulting volume in VGSTUDIO MAX, quantifying porosity, wall thickness, and deviation from a CAD model. The course closes with the applications that justify a CT investment beyond pass/fail inspection — process optimization, dimensional metrology, feedstock and lattice evaluation, powder metallurgy parts, and CT paired with destructive metallography in failure analysis — and with a frank treatment of the method's limits, including where CT measurement is not yet traceable.

Content is drawn from the *ASM Handbook* series, including Volume 17 (*Nondestructive Evaluation of Materials*) and Volume 24A (*Additive Manufacturing Design and Applications*). This is the ideal class for anyone who inspects, specifies inspection for, or is evaluating the purchase of industrial CT for metal parts.

Who Should Attend?

  1. Quality and NDT engineers responsible for inspecting additively manufactured components
  2.  Additive manufacturing engineers and process developers
  3. Metallurgists and materials engineers working in characterization or failure analysis
  4. Design engineers who specify inspection requirements for metal parts
  5.  Powder producers and feedstock quality personnel
  6. Laboratory managers and technical buyers evaluating an industrial CT purchase

Learning Objectives

Upon completion of this course, you should be able to:

  • Position computed tomography and radiography within the nondestructive testing toolkit, and recognize where conventional methods are defeated by the geometry and surface finish of additively manufactured parts
  • Specify a CT system class and scan parameters — voltage, filtration, current, exposure, frame averaging, and projection count — from the voxel size the inspection question demands
  • Diagnose beam hardening, streaking, ring artifacts, field-of-view truncation, and scatter
  • Acquire and reconstruct a CT scan, then segment the volume to quantify porosity, and wall thickness
  • Apply CT beyond pass/fail inspection to process optimization, dimensional metrology, feedstock and lattice evaluation, and correlative metallography in failure analysis
  • Evaluate the limits of the method — resolution versus part size, penetration by material, and contrast blind spots— when specifying or reviewing a CT inspection

IACET CEU's will be awarded for successful completion of the course requirements.

Course Outline:

      1. Nondestructive Testing Foundations: Where Radiography and CT Fit
      2. Radiography, X-Ray Sources, and Radiation Safety
      3. CT Physics, Reconstruction, and System Classes
      4. Image Quality, Dose, and Artifact Diagnosis
      5. Laboratory Session: Scanning an Additively Manufactured Component
      6. Porosity Quantification, Segmentation, and Dimensional Metrology
      7. Applications Beyond Pass/Fail: Feedstock, Lattices, Powder Metallurgy, and Correlative         Metallography

Continuing Education Units: 1.3

Location

9639 Kinsman Rd
Novelty, OH 44072-9603