  • 1.  Potential in Pourbaix Diagrams

    Posted 29 days ago

    Dear All,

    I would appreciate your help with the following questions

    1. Is the potential in a Pourbaix diagram measured always relative to a standard reference such as the SHE?

    2. Could you recommend a text or paper to read about this?

    Thanks,

    Wentao



    ------------------------------
    Wentao Qin
    Engineer
    On Semiconductor
    Phoenix AZ
    ------------------------------


  • 2.  RE: Potential in Pourbaix Diagrams

    Posted 28 days ago
    Wentao,

    The Pourbaix diagrams are in reference to Equilibrium Potential Eo and pH.

    They only offer a thermodynamic description of the metal-solution system, that is to say: a material corrodes or does not corrode, or it is passive or not passive or finally: it remains immune or not. They indicate the final state of the system, but do not mention the speed with which this state is reached.

    It will not tell you anything about kinetics, that is, the speed at which corrosion will occur.

    A very interesting book is: Corrosion and Protection, by Einar Bardal (2003), (Springer)

    Regards,

    ------------------------------
    [Patricia Silvana] [Carrizo]
    [Ms.]
    [Chemical Engineer]
    [Archaeometallurgy Area - UTN FRM]
    [Mendoza] [Argentina]
    [+542615577229]
    ------------------------------



  • 3.  RE: Potential in Pourbaix Diagrams

    Posted 28 days ago

    Thank you Patricia.

    Could you share what the definition of E0 is?

     

    Thanks,

     

    Wentao






  • 4.  RE: Potential in Pourbaix Diagrams

    Posted 28 days ago
    Wentao Eo is the potential in equilibrium of the reaction.


    ------------------------------
    [Patricia Silvana] [Carrizo]
    [Ms.]
    [Chemical Engineer]
    [Archaeometallurgy Area - UTN FRM]
    [Mendoza] [Argentina]
    [+542615577229]
    ------------------------------



  • 5.  RE: Potential in Pourbaix Diagrams

    Posted 28 days ago

    HI Patricia,

     

    Let me read the book you recommend first.

     

    Thanks,


    Wentao






  • 6.  RE: Potential in Pourbaix Diagrams

    Posted 27 days ago
    I think the article https://en.wikipedia.org/wiki/Pourbaix_diagram is a good intro.

    ------------------------------
    Brian Berg
    Sr. Research Fellow
    Boston Scientific
    St Paul MN
    7634942677
    ------------------------------



  • 7.  RE: Potential in Pourbaix Diagrams

    Posted 26 days ago
    Thank you Brian and Patricia. I am glad. I will get back on this subject.

    Wentao

    ------------------------------
    Wentao Qin
    Engineer
    On Semiconductor
    Phoenix AZ
    ------------------------------