I took a quick look in the
ASM Medical Materials Database. It has listings for five specific grades of Polyamide 66 (Nylon 66):
- ColorRx NY2-1000RX (Conditioned)
- ColorRx NY2-1000RX (Dry)
- Zytel 42A NC010
- Zytel SC310 NC010 (Dry)
- Zytel ST801 NC010
The database notes that these grades are marketed as being suitable for medical applications.
The supplier for the ColorRx grades is listed as LTL Color Compounders, Inc. The supplier for the Zytel grades is listed as DuPont, Inc.
I hope this helps!
------------------------------
Scott Henry
Senior Content Engineer
ASM International
Materials Park OH
------------------------------
Original Message:
Sent: 01-29-2021 09:43
From: Adrian McMahon
Subject: Medical Grade Nylon 66 Supplier
Hi all,
Would anyone be able to connect me with a supplier willing to supply Medical Grade Nylon 66 for a project here in Ireland.
Early stage prototyping in progress with standard and food grade materials, but need to move to Medical Grade.
Thanks in advance!
Adrian
------------------------------
Adrian McMahon
Principal R&D Engineer
Galway
+353 (087) 400-8363
------------------------------