Hi Debbie
I am not sure if the client mean the deformation in the axial direction relative to that of the lateral one which he calls "reduction". If this is the case, the ratio between them is about 3 for most metals. This is the Poisson ratio . This means the intrusion rate is 3 times the reduction rate in the elastic mode of deformation..
Waleed Khalifa.
------------------------------
Waleed Khalifa
Professor of Metallurgical Engineering
Cairo University, Faculty of Engineering
Maadi, Cairo
01098163293
------------------------------
Original Message:
Sent: 07-24-2020 09:05
From: Debbie Peterson
Subject: Intrusion Rate of Stainless
Good Morning,
I have a customer asking if the intrusion rate is 2x the reduction rate failure for two of our stainless products (Custom 450 and LDX2101). This is not something I am familiar with and could not really find any information on. Would anyone be able to help?
Thanks,
------------------------------
Debbie Peterson
General Manager
Associated Steel Corporation
Cleveland OH
2164087627
------------------------------