    I would like to know what all the process parameters that influence the case depth of Gaseous Nitro carburized layer.
    In order to get 20 microns case depth (white layer )what are the typical values of Temperature Time and kn value or nitriding potential to be maintained.
    Please share your experience.
    Sampathkumar
    Chennai 


  • 2.  RE: Gaseous Nitrocarburizing

    ASM Employee
    Posted 29 days ago
    Perhaps @Jack Kalucki could help. He was the coauthor of this ASM HB article:

     

    K.-M. Winter, J. Kalucki, Gas Nitriding and Gas Nitrocarburizing of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 647–679, https://doi.org/10.31399/asm.hb.v04a.a0005806

    ​​

    ------------------------------
    Carrie Hawk
    ASM International
    Community Engagement Specialist

    440-338-5497
    carrieh@asminternational.org
    ------------------------------



  • 3.  RE: Gaseous Nitrocarburizing

    Posted 28 days ago
    It would be important to know what the alloy is.

    ------------------------------
    Ken Kirby
    Snap-on, Inc.
    Kenosha WI
    (262) 748-3836
    ------------------------------



  • 4.  RE: Gaseous Nitrocarburizing

    Chennai Chapter Admin
    Posted 28 days ago
    low carbon steel  (1010-10180)
    medium carbon steel (1045-1050)
    Medium Carbon Alloy steel (4140)

    N.Sampathkumar
    MD
    Ambattur Metal Treaters 
    1/A1 SIDCO INDUSTRIAL ESTATE 
    AMBATTUR 
    CHENNAI 600098
    Mobile:9841035501
    GST NO :33AADPK3898F1ZN

    N.Sampathkumar
    Co-Chairman -6ThACHTSE 2020 Chennai
    Vice Chairman -ASM international Chennai chapter 
    1/A1 SIDCO Industrial Estate,
    Ambattur,Chennai -600098
    asmicc12@gmail.com
    GST No:33AAGAA0488F1Z1 






  • 5.  RE: Gaseous Nitrocarburizing

    Posted 27 days ago
    In the case of low carbon steels, why do you want nitriding? Do you have wear problems? You should go to nitrocarburizing

    ------------------------------
    Donato FIRRAO FASM
    Professor
    Politecnico di Torino
    TORINO
    +393351494032
    Italy
    ------------------------------



  • 6.  RE: Gaseous Nitrocarburizing

    Chennai Chapter Admin
    Posted 27 days ago
    Thanks for your respose.
    I was refering to Nitrocarburizing only.
    We all know that Nitriding is preferable for Cr and Al alloyed steels only.
    I would like to know the nitriding potential as applicable for nitrocarburizing of low,Medium,carbon and alloy steels.