ASM Online Member Community

Join Puget Sound Chapter ASMI Trustee Presentation May 4th - "Wire-Fed Electron Beam Additive Manufacturing of Ti6Al4V", Dr. Priti Wanjara, FASM. See "Event Details" at our web address: https://connect.asminternational.org/pugetsoundchapter/home

  • 1.  Join Puget Sound Chapter ASMI Trustee Presentation May 4th - "Wire-Fed Electron Beam Additive Manufacturing of Ti6Al4V", Dr. Priti Wanjara, FASM. See "Event Details" at our web address: https://connect.asminternational.org/pugetsoundchapter/home

    Puget Sound Chptr Admin
    Posted 04-27-2021 21:36

     Greetings All,

    Please join us on Tuesday, May 4 at 5:15 Pacific Time (PT) for the Puget Sound Chapter ASMI Trustee presentation - - "Wire-Fed Electron Beam Additive Manufacturing of Ti6Al4V", Dr. Priti Wanjara, FASM.  

    Networking 5:15 PM, Presentation 5:30 PM, Cost: Free. (All times in PT)
    Location: Virtual meeting with RingCentral:
    Please RSVP by email to psasmnewsletter@gmail.com/" target="_blank" rel="noopener">psasmnewsletter@gmail.com.  The Ring Central Link with be sent to you upon receipt of the RSVP.
     

    Title: WIRE-FED ELECTRON BEAM ADDITIVE MANUFACTURING OF Ti6Al4V

    Dr. Priti Wanjara, FASM
    Principal Researcher and Manager
    National Research Council of Canada Aerospace
    Montreal, Quebec, CANADA

    ABSTRACT: The manufacturing technologies in industry are rapidly evolving into factories of the future with the advent of additive manufacturing technologies. Presently, the status-quo in research for metal additive manufacturing is centered on the fabrication of small parts with optimization performed for weight savings and performance using mainly laser powder-bed 3D printing technology. For the production of large parts, such as those that are likely to be used in aircraft engines, air frame structures or other large mechanical systems, the manufacturing approach entails migrating to higher deposition rate 3D printing. In this regard, wire-fed electron beam additive manufacturing (EBAM) is gaining momentum as an enabling technology for the fabrication of near net shape metallic components through a rapid layer by layer deposition process. Specific advantages of the EBAM process are the relatively large build envelop – that becomes infinite for in-space production – combined with the near 100% material efficiency of the wire-feed into the melt pool and high bulk material deposition rates of 200-600 mm3/s depending on feature size and material. Work on the EBAM process at the National Research Council of Canada (NRC) has strived to address the different underlying challenges presently facing the global scientific and research communities for introducing, producing and qualifying materials and structures fabricated through a hybrid additive subtractive approach, as compared to a subtractive methodology. This presentation highlights the advancements in the EBAM technology for depositing titanium alloy Ti6Al4V. The presentation covers the characteristics of EBAM Ti6Al4V deposit in terms of the microstructure, residual stresses, distortion, microhardness, static tensile properties, low and high cycle fatigue properties under uniaxial loading, as well as high cycle vibration fatigue behavior. Fractographic analysis after tensile and fatigue testing, as well as fatigue crack path analysis point to the importance of the alpha-beta microstructural features in EBAM Ti6Al4V

    BIO:  Dr. Priti Wanjara is Principal Researcher and Manager at the National Research Council of Canada. She earned her B. Eng (1993) and Ph.D. (1999) degrees from McGill University in Metallurgical and Materials Engineering. She started working for the National Research Council of Canada (NRC) in 2002 in the Aerospace division. Throughout her career, she has been concerned with the physical metallurgy of metals/alloys, and in particular with how this knowledge can be applied to welding process design for advanced manufacturing in the aerospace, automotive and power generation industries. Her work has emphasized the understanding of solidification and microstructural phenomena during welding of various aluminum-, magnesium-, iron-, zirconium, nickel- and titanium-based materials. Her most significant research contributions include her pioneering work on electron beam additive manufacturing, linear friction welding and friction stir welding (FSW), which has accelerated fabrication and refurbishment improvements of various components for various small medium enterprises, original equipment manufacturers and maintenance repair and overhaul industries. Dr. Wanjara is the author or co-author of over 200 papers published in refereed journals or conference proceedings and 100 NRC reports. She is recognized internationally as a leading material scientist in advanced manufacturing technologies, and is a Fellow of ASM International, the Canadian Institute of Mining, Metallurgy and Petroleum (CIM) and the Canadian Welding Bureau. She has also been awarded the ASM Silver Medal, ASM Canada Council Brian Ives Lectureship and G MacDonald Young Award, as well as the Queen Elizabeth II Diamond Jubilee Medal from the Government of Canada for her contributions to materials processing technology. Within ASM, Priti has been a contributing member for 25 years (starting as a student volunteer in 1993) with service as an executive member of the Montreal Chapter for 17 years and Chapter Chair from 2008-2013. She has also served on several Society Councils and Committees of ASM. 



    ------------------------------