Eli,
Some data for Invar is provided in the following article
Low-Expansion Alloys,
Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 665–667,
https://doi.org/10.31399/asm.hb.mhde2.a0003159Access is free for ASM Members.
Some data from various commercial producers are provided in
Alloy Digest data sheets. Here's a
list of the sheets that may have relevant data.
------------------------------
Scott Henry
Senior Content Engineer
ASM International
Materials Park OH
------------------------------
Original Message:
Sent: 08-31-2021 01:48
From: Eli Yudkevich
Subject: INVAR 36
Looking for information :
Uni axial tensile test in the longitudinal, diagonal and transverse directions. Preferably the raw data. If not available, hardening curve in the longitudinal direction.
Thank you
------------------------------
Eli Yudkevich
consultant engineer
self employ
kfar saba il
972 523663911
------------------------------