ASM Online Member Community

Expand all | Collapse all

Physical Properties of Alloy C95500

  • 1.  Physical Properties of Alloy C95500

    Posted 5 days ago

    I would be thankful if you could suggest a reference where I could obtain the following temperature dependent properties of the subject alloy:

    1. Thermal expansion
    2. Thermal conductivity
    3. Thermal diffusivity
    4. Modulus of elasticity
    5. Possson's ratio
    6. Density

     

     

    Thanks

    Dipak Chandiramani



  • 2.  RE: Physical Properties of Alloy C95500

    Posted 5 days ago

    Hi Dipak,
    Please check the following link ;
    https://alloys.copper.org/alloy/C95500



    ------------------------------
    Mohamed Alshwigi
    Materials Science PhD Student
    Wayne State Univ
    Westland MI
    (313) 615-9509
    ------------------------------



  • 3.  RE: Physical Properties of Alloy C95500

    Posted 4 days ago

    Thank you, Mohamed.

    I am however looking for variation in each of these properties with temperature.

    Thank you once again for your help.






  • 4.  RE: Physical Properties of Alloy C95500

    Posted 4 days ago
    Perhaps someone in the ASM Online Community can confirm whether or not the temperature dependency of some of the properties is included in the ASM Alloy Center Database.
    ASM Alloy Center Database™ - ASM International
    https://www.asminternational.org/materials-resources/online-databases/-/journal_content/56/10192/15468704/DATABASE

    ------------------------------
    Phillip Johnson
    Daikin Applied
    Staunton VA