Anyone having information that can be shared about the causes for the contaminated powder produced by HMI Metal Powders between ...
Silicon has a mild effect on hardenability and a moderate effect on annealability. Please see the attached two papers that I ...
Hello Robert I will like to learn more of thermal spray powder to repair hydraulic cylinder Awaiting your kind guidance ------------------------------ ...
Just to build on Parik's assessment…. I agree that "Sandblasting" is just one option. It's typically used as a surface ...
Hello Nayan, You may want to take a look at the ISTFA Conference Proceedings, https://www.asminternational.org/edfas/technical/proceedings/. ...
Many Thanks Vicky for sharing this biography! And Happy Women Day to all the STEM Women!! Kind Regards ------------------------------ ...
It's been several decades but the mnemonics still work - Prof. Honegger taught us that when it comes to interstitials in iron, ...
The time has come to start expressing the findings we are seeing and testing when it comes to thermal growth alloy properties, ...
Are there any industry standards or regulatory requirements for the marking of anodized aluminum products? Similar to the hallmarking ...
Hi Diane, Please also give it try to MetLab Corporation. I bought few equipment for our plant from them in the past and working ...