Dear Members
Required results are :
1. Surface Hardness
850 Hv 0.32. Diffused Layer
100 Microns3. White Layer
50 Microns4.Material Specifications IS 513Thickness 2.0mm
5. Finish
Chrome Color or Silver Color
Please Suggest whether should we opt for Gas Nitriding or Gas Carbourising.Also let me know if someone could achieve the same Finish for us.
Hoping for a good response from the members
Regards
Arjun Aggarwal
Aggarwal Concast Private Limited
+91 99887-16882
------------------------------
RAJESH AGGARWAL
Director
AGGARWAL CONCAST PVT LTD
ludhiana
(931) 691-6882
------------------------------