    Surface hardened helical gears must survive in harsh environments, so the heat treatment must produce the desired microstructure and material properties. Many companies use hardness testing to verify their carburizing, nitriding, and induction hardening processes.

    In this webinar, attendees will learn about the possible uses and limitations of:

    • Vickers: CHD, Nht, and Rht
    • Knoop: Nitrided or decarburization layer
    • Rockwell: Jominy testing
    • Area mapping to visualize heat treatment results

     

    Biography:

    Kelsey Torboli is a graduate of The Ohio State University, with a B.S. in materials science and engineering. Previously a metallurgist with the ESM Group Inc., she is currently an applications engineer with Struers Inc., and is a member of the ASM Cleveland Chapter as well as the ASM IDEA Committee. When she's not working in the lab or assisting customers, Kelsey enjoys Orangetheory Fitness, running in the Cuyahoga Valley National Park, and practicing and teaching at the Karate-Do Academy where she holds the rank of Black Belt.



    ------------------------------
    Carrie Hawk
    ASM International
    Community Engagement Specialist

    440-338-5497
    carrieh@asminternational.org
    ------------------------------
    Media Kit


  • 2.  RE: Hardness Testing for Heat Treaters - Free Webinar

    Posted 07-24-2022 10:01

    Reminder

    Struers webinar July 26 at 2:00 PM ET

    REGISTER HERE

    Title: Hardness Testing for Heat Treaters

    Speaker: @Kelsey Torboli, Applications Engineer, Struers Inc.



    ------------------------------
    Carrie Hawk
    ASM International
    Community Engagement Specialist

    440-338-5497
    carrieh@asminternational.org
    ------------------------------
    Media Kit