    Dear Thermal Spray Community!

    The most recent NRC paper on APS YSZ TBCs was just published in the Journal of Thermal Spray Technology (JTST) of ASM-TSS.

    The paper is entitled "Porous APS YSZ TBC Manufactured at High Powder Feed Rate (100 g/min) and Deposition Efficiency (70%): Microstructure, Bond Strength and Thermal Gradients".

    This is an open access (i.e., free download) paper.

    To download the PDF file into your computer, just click here: https://link.springer.com/article/10.1007/s11666-021-01302-y

    Cheers!

    ------------------------------
    Rogerio Lima, PhD
    Senior Research Officer
    National Research Council of Canada
    ASM Thermal Spray Society (TSS) Vice President
    ------------------------------