Dear John,
Its mean not a hard chrome but it's a replacement of hard chrome, As described by Masih above it's generally Tungsten Carbide Coating applied by HVOF thermal spray process and Ceramic ChromeOxide-Cr2O3 Coating applied by APS process.
All content which has Cr and WC are known as carcinogenic powder as Cr become hexavalent chrome after atmospheric oxidation which is define as carcinogenic powder. But you may refer MSDS of powder for better understanding of use.
Kind Regards
Chirag Raval
------------------------------
Chirag Raval - M.Engg. in Met. & Mate. Engg.
Thermal Spray Applications & Know How Technology Transfer
chirag.ase@gmail.com
------------------------------
Original Message:
Sent: 07-03-2022 03:04
From: Masih Ghorbanalinejad
Subject: HCRP thermal spray
Hi John,
HCRP = Hard chrome replacement
It means you have to use a wear resistant coating which is not hard chrome plating.
WC HVOF coating or Cr2O3 are among the most famous replacements of Hard chrome plating.
Regards,
------------------------------
Masih Ghorbanalinejad
Thermal Spray Specialist
NORTHWEST METTECH
Surrey BC
+1 604 704 0637
Original Message:
Sent: 07-01-2022 11:33
From: John Merrill
Subject: HCRP thermal spray
A specification calls for HCRP wear resistant coating to a 304 stainless steel surface. I cannot find a definition of HCRP. Chrome oxide HVOF and plasma are popular in our industry, so could it be hexavalent chromium free plasma?
------------------------------
John Merrill
Principal Engineer
EagleBurgmann
Matthews NC
7048407045
------------------------------