Principles of Failure Analysis, 3 day, September 14-16, 2026

When:  Mon, Sep 14, 2026 from 08:30 to 16:30 (ET)

This lecture course is designed to provide the knowledge to bridge the gap between theory and practice of failure analysis. This course presents a very practical approach to failure analysis for those who are new to the field or those who want an update. It is also designed for technicians with the prerequisites and those interested in understanding how knowledge of failure analysis can lead to better productivity. Causes of fractures are explained with diagrams of stress application and distribution. Many case histories of failures and their elimination are highlighted throughout the course.

WHO SHOULD ATTEND:

  • Degreed engineers who are new to failure analysis or seeking an update
  • Technicians with at least five years of full-time experience in a failure analysis lab who can prepare and interpret microstructures and perform basic mechanical tests

LEARNING OBJECTIVES:

Upon completion of this course, you should be able to:

  • Describe general procedures, techniques and precautions in failure analysis
  • Recognize how stress systems relate to fracture of ductile and brittle materials
  • Identify typical fatigue, wear, corrosion and elevated-temperature failure characteristics

COURSE OUTLINE:

  1. General Procedures for Failure Analysis
  2. Fatigue Failures
  3. Wear Failures
  4. Corrosion Failures

Continuing Education Units: 2.0