EDFAS Online Community

 View Only
  • 1.  X-ray fluorescence (XRF) Spectometry Tools

    Posted 05-11-2021 14:04
    Hello EDFAS,

    Over the past few years, my colleagues have used XRF as a first-cut method to assess lead finish composition on packaged devices.  Doing this frees up our SEM/EDS for more intensive investigations.  This made me want to examine the universe of XRF tools in more detail.  So I'd like to pose the following questions to the community to gauge your personal experiences:

      > Do you use XRF frequently?  In what applications do you find it most useful?
      
      > What tool/features do you like the best?  (no need to cite brand names if you do not wish to)

      > What drawbacks have you seen using the XRF tools at your disposal?

      > In your experience how does XRF compare to other material analysis methods?

    I'm looking forward to seeing your comments in these areas.

    Cheers,
    --- Ted K.

    ------------------------------
    Ted Kolasa
    Engineer
    Northrop Grumman
    Chandler AZ
    ------------------------------
    Register for an upcoming course with ASM International


  • 2.  RE: X-ray fluorescence (XRF) Spectometry Tools

    Posted 05-26-2021 15:59
    Here is a link to some papers relating to XRF in the ASM Digital Library--ISTFA proceedings. As a member, you should have access to these in your "My Content".

    I would also refer you to @S.h. Lau who may be able to help you.


    ​​​​

    ------------------------------
    Carrie Hawk
    ASM International
    Community Engagement Specialist

    440-338-5497
    carrieh@asminternational.org
    ------------------------------

    Register for an upcoming course with ASM International


  • 3.  RE: X-ray fluorescence (XRF) Spectometry Tools

    Posted 05-26-2021 16:08
    @Joe Colangelo might be someone else that could help with this inquiry.


    ------------------------------
    Carrie Hawk
    ASM International
    Community Engagement Specialist

    440-338-5497
    carrieh@asminternational.org
    ------------------------------

    Register for an upcoming course with ASM International