  • 1.  AISI 316

    Posted 11-19-2021 02:18
    I am wondering if there is different between AISI 316 and AISI 316 Anneald ? ( as per AMS5524 )

    ------------------------------
    Eli Yudkevich
    consultant engineer
    self employ
    kfar saba il
    972 523663911
    ------------------------------
    IMAT 2022 - Registration Now Open


  • 2.  RE: AISI 316

    Posted 11-20-2021 06:16
    I don't have a copy of AMS5524 available to me.  But many production specs of alloys (for instance just calling out AISI 316, or the equivalent UNS number, or certain ASTM specs) specify only the chemical analysis limits and not heat treatment condition.  Type 316 is available in various conditions and strength levels from cold work.  If someone specifies annealed then usually it means solution annealed for which there are cooling time/temperature limits to guarantee the part is not sensitized, which reduces corrosion resistance.  If solution annealed the strength will be at the lowest available in the alloy as all cold work will have been removed.  If the material has been heated or cold rolled then it no longer counts as annealed, unless the final step is a solution anneal. 

    I hope that this is helpful information.  It is usually best to have a copy of the relevant year revision of the referenced specification which can be purchased online from SAE or other sources for less than the cost of an hour of engineering time.



    IMAT 2022 - Registration Now Open


  • 3.  RE: AISI 316

    Posted 11-20-2021 23:25

    Thank you for your reply !

     

     

    Eli  Yudkevich

           Consultant 

      Aerospace manufacturing

              spacialist

     

    Phone: 972 9 7424084 

    Mobile: 972 52 3663911

    Email: eyudkevich@gmail.com

     

    Kfar-Saba 4428636

            ISRAEL

     

    www.eliyudkevich.com

     

    Title: LinkedIn - Description: image of LinkedIn icon 

     

     

     




    IMAT 2022 - Registration Now Open