Folks -
I would appreciate any feedback on plastometry.
See the attached article from the recent AMP.
Profilometry-Based Indentation Plastometry
Brings Speed and Accuracy to Metallurgical R&D.
April 2022, p19
More info on the vendor's web page:
https://plastometrex.com/and YouTube including this intro video:
Intro to PLX and Indentation Plastometryand:
Plastometrex
YouTube |
remove preview |
|
Intro to PLX and Indentation Plastometry |
Introductory video to Indentation Plastometry and Plastometrex from CEO James Dean |
View this on YouTube > |
|
|
thanks and kind regards,
- Jim
PS: This is not an advertisement. I am seriously interested in chatting
with any users of this equipment and/or technique.
------------------------------
Jim Quinn
Stony Brook University
Stony Brook NY
------------------------------