TSS Membership Community

 View Only

ASM-TSS TS4E 2023 - in less than two weeks

  • 1.  ASM-TSS TS4E 2023 - in less than two weeks

    Posted 09-01-2023 12:55

    Dear Thermal Spray Community!

    This is the list of amazing speakers of the ASM Thermal Spray Society (TSS) event Thermal Spray of Suspensions & Solutions Symposium + EBCs (TS4E 2023), to be held at the University West (Sweden) on September 12-13 (2023):

    Bryan Harder, NASA (USA): Thermal Spray Processing and Testing of Advanced Environmental Barrier Coatings

    Robert Vaßen, Jülich RC (Germany): Recent Results on Suspension Plasma Sprayed Thermal Barrier Coatings (TBCs)

    Tom Coyle Coyle, University of Toronto (Canada): Control of Coating Structure in Solution Precursor Plasma Spray

    Nicholas Curry, Mettech (Canada): Suspension Plasma Spray - Where Are The Limits?

    Jonathan Gutleber, Oerlikon Metco (USA): CMAS Resistant TBCs Deposited using Suspension Plasma Spray

    Professor Tanvir Hussain, University of Nottingham (UK): Next Generation of Microstructure & Composition from Axial injection SPS for Aerospace Propulsion: Artificial intelligence & Thermo-Chemico-Mechanical Assessment

    Mohit Gupta and Shrikant Joshi, University West (Sweden): Hybrid Powder-Suspension Thermal Spray Coatings: The Way Forward?

    Barbara Maroli, Hoganas (Sweden): Silicon and Rare Earth Silicate powders for EBCs

    Christian Moreau Concordia University (Canada): Materials Synthesis and Modification in Suspension Plasma Spray

    Radek Musalek, Institute of Plasma Physics (Czech Republic): High-Throughput Plasma Spraying of Multiphase Coatings with Liquid Feedstocks

    Yoshifumi Okajima, Mitsubishi Heavy Industries (Japan): Comparative Study of Thermal Barrier Coatings by S-HVOF, S-APS AND EB-PVD Processes

    Lisa Pin, Safran (France): Enhanced EBC Development and Behaviour Analysis for High Temperature CMC Components

    Vincent Rat, University of Limoges (France): Current Plasma Torches for Suspension Plasma Spraying: Features, Modelling and Diagnostics

    Jim Ruud, GE Global Research Center (USA): Suspension Thermal Spray Technologies

    Sanjay Sampath, Stony Brook University (USA): Fundamental Issues in Plasma Spraying of Silicate Environmental Barrier Coatings

    Kentaro Shinoda, AIST (Japan): Alternate Route for Spray Deposition of Fine Particles to Fabricate Dense Ceramic Coatings and its Application to Environmental Barriers

    Paweł Sokołowski, Wroclaw University (Poland): Improving the Self-Healing Abilities of TBCs by Using Complex Thermal Spray Concepts

    Richard Trache, Treibacher Industrie (Austria): The Different Feedstocks for Thermally Sprayed EBCs

    Jingyang Wang, Institute of Metal Research, Chinese Academy of Sciences (China): Strategic Advancements on Environmental Barrier Coatings for SiCf/SiC Composite

    Dapeng Zhou, Julich RC (Germany): Environmental Barrier Coatings Deposited by Suspension Plasma Spraying

    Simone Bursich, Lincotek (Italy): Properties of Suspension Sprayed Thermal Barrier Coatings Deposited by Advanced Cascaded Plasma Spray Technology

    The TS4E 2023 website: TS4E 2023 (asminternational.org)

    See you all there!



    ------------------------------
    Rogerio Lima, PhD
    Senior Research Officer
    National Research Council of Canada
    Fellow of ASM International (FASM)
    President of Thermal Spray Society (TSS)

    e-mail: rogerio.lima@nrc-cnrc.gc.ca
    ------------------------------