    Now through the end of June, the Journal of Thermal Spray Technology review article "Advancements in Deposition of High Entropy Alloys Using Cold Spray Technology" by Magesh Kumaravel, Sara Bagherifard, and Mario Guagliano is free access for you to download and read!

    This review is aimed at providing a detailed state of the art of cold-sprayed high entropy alloys (HEAs). The microstructure evolution after cold spray, as well as the function and performance in terms of wear resistance, mechanical strength, corrosion resistance and oxidation resistance of the deposits are discussed for all cold spray deposits of HEAs. The reported post-treatments applied to HEAs deposits and their effects on functionality are also discussed to help us lay a base for further investigations and developments in the new horizon of HEAs. Perspectives on potential future developments are discussed to provide directions for research investigations in the field of cold spraying of HEAs.

    To read the article, please visit here now through June 30th.



    ------------------------------
    Emily Glorioso
    ASM Employee
    ASM International
    Novelty OH
    (440) 338-5151
    ------------------------------
    Register for an upcoming course with ASM International