Original Message:
Sent: 06-03-2022 09:14
From: Rogerio Lima
Subject: Thermal spray coatings for food contact
Fantastic Chirag,
FYI - @ the TSSE 2022 we (thermal sprayers) will have a dedicated TSS networking area within the exposition, where we will have the (i) coffee-breaks, (ii) lunches, (iii) table tops and (iv) a poster competition for Emerging Professionals (graduate students and post-docs). Everything related to thermal spraying. Therefore... the networking will likely be intense :)
The agenda of the TSSE 2022 can be found here: e1da5939-6033-8140-7125-8d0a715f0b95 (asminternational.org)
The registration for the TSSE 2022 is now open: Registration - TSS Forum (asminternational.org)
If I do not have any professional commitment at the NRC in that week, for sure I will be Thermal Spray & Surface Engineering Forum & Expo 2022 (TSSE 2022).
And it will be a pleasure to meet you (and everybody else) F2F @ the TSSE 2022.
Cheers!
------------------------------
Rogerio Lima, PhD
Senior Research Officer
National Research Council of Canada
ASM Thermal Spray Society (TSS) Vice President
------------------------------
Original Message:
Sent: 06-03-2022 07:39
From: Chirag Raval
Subject: Thermal spray coatings for food contact
Yes this is very good platform to discuss technical and new developments things for all thermal spray learner, beginner and experts.
Thank you so much Rogerio. I'm looking forward to it.
May be we can meet soon in US. I'm planning to attend Thermal Spray & Surface Engineering Forum & Expo in September.
------------------------------
Chirag Raval
Thermal Spray Applications & Know How Technology Transfer
chirag.ase@gmail.com
Original Message:
Sent: 06-03-2022 07:04
From: Rogerio Lima
Subject: Thermal spray coatings for food contact
Dear Chirag,
It is an honour to have you and dozens of thermal sprayers within this group. It is a great opportunity to all of us to ask technical questions and share technical information related to thermal spraying.
Just like you... there are many thermal spray experts in here.
And regarding your willingness to serve as volunteer to TSS... you are very welcome... it is noted... and I got your email.
Cheers!
------------------------------
Rogerio Lima, PhD
Senior Research Officer
National Research Council of Canada
ASM Thermal Spray Society (TSS) Vice President
Original Message:
Sent: 06-03-2022 03:14
From: Chirag Raval
Subject: Thermal spray coatings for food contact
Dear Rogerio
It's my pleasure to be part of this group.
let me know if any volunteers opportunities their for me in ASM TSS group.
I'll be more than happy to explore it.
Thanks and Regards
------------------------------
Chirag Raval
Thermal Spray Applications & Know How Technology Transfer
chirag.ase@gmail.com
Original Message:
Sent: 06-02-2022 17:46
From: Rogerio Lima
Subject: Thermal spray coatings for food contact
Dear Chirag,
Thanks for letting us know.
It is always good when someone can provide some feedback regarding an info available on a website.
Your feedback is highly appreciated.
Cheers!
------------------------------
Rogerio Lima, PhD
Senior Research Officer
National Research Council of Canada
ASM Thermal Spray Society (TSS) Vice President
Original Message:
Sent: 06-02-2022 07:43
From: Chirag Raval
Subject: Thermal spray coatings for food contact
Hi Milad, Rogerio
Based on my perspective and considering safety Cr2O3 is considered as a carcinogenic material. All that powder which content with Chromium are considered carcinogenic powder in thermal spray.
it's become hexavalent chrome after oxidation which is not good for direct food contact applications.
-
Kind Regards
Chirag Raval
------------------------------
Chirag Raval
Sr. Er. Applications - Thermal Spray
Oerlinon Surface Solutions
Original Message:
Sent: 05-29-2022 20:41
From: Milad Rad
Subject: Thermal spray coatings for food contact
Hi Rogerio,
Thank you for this great question. Thermal-sprayed chromium oxide (Cr2O3) and chromium carbide (Cr3C2) coatings have been mentioned on the websites below as FDA-compliant coating solutions for food processing applications. According to the information provided on these websites, thermal spray coatings can provide high resistance against corrosion for parts exposed to acidic solutions and foodstuff residues. Please take a look at the following websites for additional information.
https://www.thermalspray.com/industries/food-and-beverage-processing/. Click or tap if you trust this link." data-linkindex="0">https://www.thermalspray.com/industries/food-and-beverage-processing/
http://www.putzier.com/en/02-applications/food-processing/food-processing.html. Click or tap if you trust this link." data-linkindex="1">http://www.putzier.com/en/02-applications/food-processing/food-processing.html
https://www.astroalloys.com/food-and-beverage.html. Click or tap if you trust this link." data-linkindex="2">https://www.astroalloys.com/food-and-beverage.html
------------------------------
Milad Rad
Assistant Professor
University of Southern Indiana
Original Message:
Sent: 05-27-2022 10:37
From: Rogerio Lima
Subject: Thermal spray coatings for food contact
Thanks Richard for the feedback;
Highly appreciated!
Rogerio
------------------------------
Rogerio Lima, PhD
Senior Research Officer
National Research Council of Canada
ASM Thermal Spray Society (TSS) Vice President
Original Message:
Sent: 05-27-2022 10:00
From: Richard Bajan
Subject: Thermal spray coatings for food contact
Hello Rogerio,
Try contacting Satish Dixit at Plasma Technology Inc. (PTI) in Torrance, CA. Years back, I knew PTI had several coatings with FDA approval.
Richard
------------------------------
Richard Bajan
National Sales Manager
IKH USA-INC.
Wellford SC