Thermal Spray Night! ASM Akron Chapter Meeting on 3/19/2025

  • 1.  Thermal Spray Night! ASM Akron Chapter Meeting on 3/19/2025

    Posted 03-10-2025 11:24
      |   view attached

    Hello All,

    Mr. Chirag Raval from Hannecard Roller Coatings Inc. will be presenting High Pressure Cold Spray Technology for Industrial Repair: Applications, Advancements, and Gas Turbine Part Case Studies. The networking hour for this meeting is being generously sponsored by Hannecard Roller Coatings (formerly ASB).

    Chirag Raval is a Metallurgist and Materials Engineering Specialist with expertise in Thermal Spray and Cold Spray processes. With over a decade of experience, he has worked in materials coatings, application development, and global technology transfer. He leads process development at Hannecard Roller Coatings Inc. and previously contributed to key projects at Oerlikon Metco. Chirag holds a Master's in Metallurgical and Materials Engineering and is actively involved in ASM International and the Thermal Spray Society.

    Abstract: High Pressure Cold Spray (HPCS) is an advanced material deposition process that restores and enhances industrial components by bonding solid powder particles through high-velocity impact without significant heating. This method produces coatings with strong adhesion and minimal thermal distortion, making it ideal for repairing gas turbine parts. This presentation explores HPCS applications in industrial repair, highlighting advancements in deposition efficiency, material selection, and coating properties. Case studies demonstrate its effectiveness in restoring critical components, improving performance, and extending operational life. The expanding role of HPCS in sustainable manufacturing and maintenance is also discussed.

    RSVP to Deborah Curtis at Deborah.Curtis@hannecard.com or 330-753-8458
    Reservations are requested no later than 3:00 pm on Friday, March 14, 2025

    Location:  New Era Restaurant, 10 Massillon Rd.  Akron, OH  44312 330-784-0087

    Networking begins at 5:00 p.m., Dinner at 6:00 p.m. Presentation 7:00 p.m.

    Cost:  $35 Members/Spouses/Retirees; $40 Non-Members/Guests; $20 Students (High School – Undergraduate). Note: Credit Cards are not accepted. Cash or check only.

    Dinner Buffet: Chicken Paprikash, Stuffed Porkchops, Potatoes, Vegetables, Salad, Coffee/Soda and Dessert.  Please specify if you require a vegetarian dinner with your reservation.

    See the attached meeting notice for additional information about Mr. Raval and his presentation. Looking forward to seeing you at the meeting!

    Cheers,
    Jen

    _____________________________________

    Jennifer Lillard, Ph.D.

    Associate Professor

    Department of Chemical, Biomolecular and Corrosion Engineering

    College of Engineering and Polymer Science

    The University of Akron

    Akron, OH 44325-3906

    She, her

    Office: 330.972.6787



    ------------------------------
    --
    Kind Regards,
    Chirag Raval - (Metallurgist & Materials Engineer)
    KEY – Thermal Spray & Cold Spray Application Specialist
    HANNECARD Roller Coatings, Inc, USA
    www.hannecardrollercoatings.com | www.asbindustries.com
    ------------------------------

    Attachment(s)