TSS Membership Community

 View Only
  • 1.  Webinar - MICROSTRUCTURE OF THERMAL SPRAY COATINGS: SAMPLE PREPARATION AND EXAMINATION

    Posted 08-11-2022 07:46
    Dear Thermal Spray Community!

    Thermal spray coatings are used in various engineering applications to provide resistance to heat (thermal barrier), wear, cavitation, abrasion, etc. Many techniques such as arc spray, high-velocity oxy fuel (HVOF), and plasma spray are available for the application of thermal spray coatings and they all basically entail the projection of molten or semi-molten droplets onto a prepared substrate where they harden and form a continuous protective coating. No matter what technique is used to apply a thermal spray coating, metallographic preparation and examination are necessary for quality control to assess coating thickness, amount and distribution of porosity, the presence of oxides and un-melted particles, as well as adhesion integrity. Incorrect grinding and polishing procedures can influence porosity results; it is therefore imperative that these steps are done in a systematic and repeatable manner.

    Please join us as Struers discusses:

    • Difficulties during sample prep and how to overcome them
    • Preparation steps: best practices for cutting, mounting, grinding and polishing
    • Methods & examples

    To register for it, just follow this post from our TS colleague Nicholas Curry: Sign Up | LinkedIn

    Cheers!

    ------------------------------
    Rogerio Lima, PhD
    Senior Research Officer
    National Research Council of Canada
    ASM Thermal Spray Society (TSS) Vice President
    ------------------------------
    Register for an upcoming course with ASM International


  • 2.  RE: Webinar - MICROSTRUCTURE OF THERMAL SPRAY COATINGS: SAMPLE PREPARATION AND EXAMINATION

    Posted 08-11-2022 07:50
    Sorry... I guess this link will work: Microstructure of Thermal Spray Coatings: Sample Preparation and Examination - Struers.com

    ------------------------------
    Rogerio Lima, PhD
    Senior Research Officer
    National Research Council of Canada
    ASM Thermal Spray Society (TSS) Vice President
    ------------------------------

    Register for an upcoming course with ASM International


  • 3.  RE: Webinar - MICROSTRUCTURE OF THERMAL SPRAY COATINGS: SAMPLE PREPARATION AND EXAMINATION

    Posted 08-11-2022 10:55
    Dear Rogerio,

    Thanks for the link. I did register for me. 

    Kind Regards,
    Chirag Raval

    ------------------------------
    Chirag Raval - (M.Engg. in Metallurgical & Materials Engineering Specialise in Material Technology)
    Thermal Spray Applications & Know How Technology Transfer
    chirag.ase@gmail.com
    ------------------------------

    Register for an upcoming course with ASM International