TSS Membership Community

 View Only

recyclers: thermal spray dusts and overspray

  • 1.  recyclers: thermal spray dusts and overspray

    Posted 05-25-2021 12:47
    I've worked with several companies who have claimed to be good at recycling thermal spray dusts and overspray materials but it still seems like there's a lot of handholding that has to be done. This became part of my R&D engineer (metallurgy/materials) a few years ago along with environmental reporting. 

    Any of you have a recycler you can recommend?

    joe
    jzanter@tstcoatings.com

    ------------------------------
    Joe Zanter
    R&D Engineer
    Thermal Spray Technologies
    Sun Prairie WI