  • 1.  Stacking faults in BCC alloys.

    Posted 03-14-2021 10:16

    Hello ASM Community,

    I am a PhD candidate working in the area of "Alloy Development using Density Functional Theory".

    Deformation mechanisms in alloys have been extensively explained with the theory of dislocation slip, twinning. When it comes to FCC alloys (ex. Austenitic SS, FCC High Entropy Alloys), stacking faults have been studied extensively. But in BCC alloys, stacking faults are not explored much.

    I am interested in knowing if there's any literature available which talks about the effect of Stacking Fault Energy in BCC alloys on their ductile-to-brittle-transition-temperature (DBTT) phenomenon.

    Thanks in advance.



    ------------------------------
    Sufyan M. Shaikh
    Dept. of Metallurgical & Materials Engineering
    Indian Institute of Technology Madras
    Tamil Nadu, India
    linkedin.com/in/sufyanshk
    ------------------------------


  • 2.  RE: Stacking faults in BCC alloys.

    Posted 03-15-2021 07:48
    The answer on ResearchGate will lead 
    you in the correct direction:
    https://www.researchgate.net/post/Why-dont-BCC-crystals-have-stacking-faults

    ------------------------------
    James Quinn
    Dir. of Laboratories
    Stony Brook University
    Stony Brook NY
    ------------------------------



  • 3.  RE: Stacking faults in BCC alloys.

    Posted 03-15-2021 08:51
    Edited by Sufyan Shaikh 03-15-2021 08:51

    Thank you Dr Quinn. I will go through those answers on Research Gate.

    I am looking for studies correlating the stacking fault energies with the ductile-to-brittle-temperature phenomenon (if there are any studies done for BCC alloys).



    ------------------------------