ASM Online Member Community

 View Only
  • 1.  Percentage Cu in 4140 alloy

    Posted 02-15-2024 10:28

    Would 0.15% Cu effect the hardness vs tempering temperature in 4140 alloy? Thanks



    ------------------------------
    Scott Wiederhold
    General Manager
    Magnum Induction Engineering
    New Baltimore MI
    586-716-4700
    ------------------------------
    ASM Education Summer Sale


  • 2.  RE: Percentage Cu in 4140 alloy

    Posted 02-16-2024 08:05
    This paper indicates that copper contents up to 0.5% have little effect: