  • 1.  Refractory High Entropy Alloy

    Posted 02-28-2023 07:33

    I am searching for tensile tests data on refractory alloys and refractory high-entropy alloys for my ongoing PhD.

    Please suggest where can I find such data websites/open-literature/public repositores/etc.

    Thanks.



    ------------------------------
    Sufyan M. Shaikh
    Metallurgical and Materials Engineering
    Indian Institute of Technology Madras
    https://sufyanshk.github.io/
    ------------------------------
    ASM Education Summer Sale


  • 2.  RE: Refractory High Entropy Alloy

    Posted 03-02-2023 14:36

    Sufyan,

    You may find some data in the following article

    S. Gorsse, M.H. Nguyen, O.N. Senkov, D.B. Miracle, Database on the mechanical properties of high entropy alloys and complex concentrated alloys,Data in Brief, Volume 21, 2018, Pages 2664-2678, ISSN 2352-3409, https://doi.org/10.1016/j.dib.2018.11.111.

    @Daniel Miracle is one of the coauthors--perhaps he can advise about other potential data sources.



    Abstract: This data article presents the compilation of mechanical properties for 370 high entropy alloys (HEAs) and complex concentrated alloys (CCAs) reported in the period from 2004 to 2016. The data sheet includes alloy composition, type of microstructures, density, hardness, type of tests to measure the room temperature mechanical properties, yield strength, elongation, ultimate strength and Young׳s modulus. For 27 refractory HEAs (RHEAs), the yield stress and elongation are given as a function of the testing temperature. The data are stored in a database provided in Supplementary materials, and for practical use they are tabulated in the present paper. The database was used in recent publications by Miracle and Senkov [1], Gorsse et al. [2] and Senkov et al. [3].

    Scott



    ------------------------------
    Scott Henry
    Senior Content Engineer
    ASM International
    ------------------------------