Posted By
Felix Beaudoin
05-11-2023 11:35
Found In
Egroup:
EDFAS Online Community
\
view thread
Dear Wentao, here are some comments from my colleague Satish Kodali. Hope this helps. Felix PVC may not always provide the answers we need to identify fails. In advanced technology nodes we have soft fails which are voltage sensitive (which we can modulate the Fail from pass to fail depending on ...
|