  • This has been an interesting discussion which I have come to just now. I don't have any experience with cold working the PH grades, ...

  • 15-5 PH and 17-4 PH are nearly identical. "Annealed" 15-5/17-4 material is untempered martensite. Consider using H1150M. -- ...

  • Most specifications are written through a consensus process, and the balance of interests (manufacturers/producers vs. users) ...

  • My specialty (failure analysis) is rare enough that I have to go where the job is. I cannot stay wedded to an individual area ...

  • I am Bernardo Servin, Engineering Manager at FRISA Forge in Mexico with 26 years of experience in the steel forging area, Mechanical ...

  • Advice to an early career materials engineer: I'd urge them to be flexible. Materials remains a rapidly evolving discipline. Young ...

  • Dear Sir/Madam, ASM International Bangalore Chapter cordially ...

  • Can anyone suggest typical Heat Treatment cycle using Ammonia flow and Nitriding potential (Kn ) controls in the following situations ...

  • The flip side though is that even if your employer does not fund or support participation, you may still gain by funding yourself ...

  • Profile Picture

    RE: Member Spotlight

    Thank you, Mark Taylor, ASM Oregon Chapter leader! @Mark Tambling specializes in welding and ferrous metallurgy. ...