Being used as weld wire, I intend to just leave 20% cold work and no further Anneal or Aging at my side. Suppling .062" Dia x ...
15-5 PH and 17-4 PH are nearly identical. "Annealed" 15-5/17-4 material is untempered martensite. Consider using H1150M. -- ...
Most specifications are written through a consensus process, and the balance of interests (manufacturers/producers vs. users) ...
My specialty (failure analysis) is rare enough that I have to go where the job is. I cannot stay wedded to an individual area ...
I am Bernardo Servin, Engineering Manager at FRISA Forge in Mexico with 26 years of experience in the steel forging area, Mechanical ...
Advice to an early career materials engineer: I'd urge them to be flexible. Materials remains a rapidly evolving discipline. Young ...
Dear Sir/Madam, ASM International Bangalore Chapter cordially ...
Can anyone suggest typical Heat Treatment cycle using Ammonia flow and Nitriding potential (Kn ) controls in the following situations ...
The flip side though is that even if your employer does not fund or support participation, you may still gain by funding yourself ...
Thank you, Mark Taylor, ASM Oregon Chapter leader! @Mark Tambling specializes in welding and ferrous metallurgy. ...