Practical Interpretation of Microstructures June 3rd-6th, 2024

events_1.jpg
Starts:  Jun 3, 2024 09:00 (PT)
Ends:  Jun 6, 2024 17:00 (PT)
Associated with  Los Angeles Chapter Community

Practical Interpretation of Microstructures 

June 3rd-6th, 2024

Dates: June 3, 2024 - June 6, 2024
VenueAllied High Tech Products, Inc.
Location: Cerritos, CA, 90703, United States
Instructor: Ms. Frauke Hogue, FASM

Course Details: This "Hands-On" course presents information on microstructures, heat treatment and use of each group of alloys. You will be able to view actual structures. The features of the structures and pointed out and discussed. You will then examine over 200 mounts at their microscope stations and compare with an illustrated and annotated notebook of the structures.
 
1. Proper Terminology for Describing Microstructures
2. Optimizing the Images on the Metallograph
3. Iron/ Carbon Phase Diagram and TTT Diagram
4. Structures of Carbon and Alloy Steels as Produced by Heat Treatments
5. Structures of Stainless Steels and Heat Resisting Alloys
6. Microstructures of Titanium and Its Alloys
7. Microstructures of Copper-Based Alloys
8. Structures of Aluminum Alloys, Cast and Wrought

For more information contact the instructor Frauke Hoguefrauke@hoguemet.com